型号: DXPMQ6.0/8.0 外观结构
标志: 表面贴荧光黄反光标贴开关: D25球阀 铜合金主体1Made of copper alloy
喷雾枪材质: 不锈钢316 冲击锤-45#(表面镀镍)
操作步骤1.Connect the hose with mist nozzle
2.Hammer tip concentrated on the certain place of the container wall. Hammer hard till the hammer tip pierces
through the container wall and take out the impact hammer. 3.Hold the mist nozzle, get the nozzle tip pass through the wall of container. If failed, hammer the nozzle end with
hammer end till the nozzle tip passes through the container wall. Then turn on the switch, start spraying to put
out the fire. Piercing ability
The hardness of tip and blade of hammer is Rockwell HRC48 ~ 56, it is easy to pierce through 2-mm-thick
试验时使用冲击锤的锤尖对准集装箱箱壁用力敲击,锤尖能完全刺穿 2mm 的 Q235A 热轧钢板,且枪尖刃部应无明factory testing, and there is no obvious damage with the tip and blade of hammer like crack, edge curl and blade
认证:RINA 
操作步骤
1.Connect the hose with mist nozzle
2.Hammer tip concentrated on the certain place of the container wall. Hammer hard till the hammer tip pierces
through the container wall and take out the impact hammer.
3.Hold the mist nozzle, get the nozzle tip pass through the wall of container. If failed, hammer the nozzle end with
hammer end till the nozzle tip passes through the container wall. Then turn on the switch, start spraying to put
out the fire.
Piercing ability
The hardness of tip and blade of hammer is Rockwell HRC48 ~ 56, it is easy to pierce through 2-mm-thick
试验时使用冲击锤的锤尖对准集装箱箱壁用力敲击,锤尖能完全刺穿 2mm 的 Q235A 热轧钢板,且枪尖刃部应无明
factory testing, and there is no obvious damage with the tip and blade of hammer like crack, edge curl and blade
认证:RINA 