Technical parameter:
Light source: LED(Flash)
Chromaticity: White
Power supply: Lithium battery
Flash Frequency: 50~70 times/min
Luminous Intensity: ≧2.0cd
Operation Life: ≧24h over 2.0cd (15h at -1℃)
Maximum Stowage Height: 76 meters
Storage Temperature: -35℃ ~ +85℃
Working Temperature: -1℃ ~ +30℃
Expiry Date: 5 years from date of manufacture
Performance: Fire-resistant, Oil-resistant, Mould-proof, Corrosion-proof, Water-proof, Dust-proof,
UV-Resisitant
Environment Performance: Meet RoHS and asbestos-free requirement
Activation: Automatically turn on when the LED lamp is upright & and water sensors contact water
simultaneously;Automatically turn off otherwise
Explosion Proof Level: II 1G Ex ia op is llC T4 Ga
Size(without clip): φ90*133mm
Weight(without clip): 180
pprove: MED EC SOLAS USCG ATEX IECEx