Liferaft Light
TYPE:YYTFD
STANDARD
SOLAS 1974/1996,LSA, MSC.81(70), MSC.36(63), MSC.48(66), MSC.97(73), MSC.200(80), MSC.266(82),MSC.323(89)
OVERALL PERFORMANCE & REQUIREMENT
Luminous Intensity: Inside light≥0.5cd Outside light≥4.3cd
Light-Duration: ≥12h
Operating Voltage: 3.6V
Light-Duration: Flashing/Always bright
Flash Frequency: 50-70 times/min
Battery: Lithium battery
The indicator light can give out light when the liferaft and boat has been inflatable

Purchase instructions
1.The site currently supports about 10 currencies, please choose the currency you want to pay.
2.For ease of purchase, buyers need only provide receipt information and email. The system will automatically send you an email notification as part of the buyer's purchase voucher.
3. If you need us to design plans for major projects such as shipbuilding, marine engineering, water restaurants, submarine entertainment, sea surfing, etc., please send a direct email to tech@dx-marine.com.
4.In order to prevent you from buying fake and inferior products, please buy it directly from our official website or call the agent and dealer.
5.On logistics: Chinese buyers acquiesced in Shentong and Yuantong. Other regions may need to ship from Hong Kong or Shanghai.