9kg dry powder fire extinguisher
Type PSMPG9
cartridge operated
Extinguishant ABC40 dry powder
Capacity (kg) 9
CO2 Gas Cartridge (g) 150
Cylinder Diameter (mm) 180
Overall Height (mm) 650
Approx Full Weight (kg) 14
Working Temp. Range -30°C to + 60°C
Test Pressure 30 Bar
Burst Pressure Exceeds 55 Bar
Approx Discharge Range (m) >4
Approx Discharge Time (sec) ≥15
Fire Rating 43A 233B C
Fire Class A B C
Cylinder Specification CE EN3-8
Discharge Assembly PVC Nozzle & Spray bucket
Mounting Wall hanger
Operating Head / Valve Brass nickel plating
Paint Finishing RAL 3000 Flame Red
Thermoset polyester
Manufactured & Certified to
CE EN 3-7 + EN 3-8
Approved MED CE EN3
Frond & back side
Bottle holder