Lifebuoy bracket
A、Technical parameter
Material:304 stainless steel、316 stainless steel、steel spraying plastics
Thickness:3mm
Certification: manufacturer certification
B、 Use
For the placement of national standard lifebuoy rings, used in 2.5kg of lifebuoy and 4.3kg lifebuoy rings or more than 700mm in diameter.
C、 Scope of use
-
For ship hanging wall;
-
Park River arrangement;
-
Sewage treatment plant hanging;
-
Water park swimming pool;
-
Decoration effect and so on.
D、 Advantage
Convenient lifebuoy rings, beautiful and generous. At the same time, the lifesaving rope can be hung so as to facilitate the suspension of the life jacket. A lot of use, save more space.