Protective clothing for fire fighting
TYPE:DXPC-1
STANDARD
SOLAS 1974, MSC.36(63), MSC.97(73), MSC.98(73), EN 469 (2005) including A1(2006) and AC (2006).
COMPRISIN:
Jacket, trousers
OVERALL PERFORMANCE & REQUIREMENT
-
Water proof: Hydraulic pressure ≥4000 Pa
-
Heat radiation resistance: Under the heat radiation with 10kw/㎡, the increase of tempeature on inner-surface not over 25℃, after irradiated for 30 seconds.
-
Material: Aramid fiber
-
Protection class: limit the fire spreading (outer material): pass
-
Limit the fire spreading (inner material): pass
-
Thermal conductivity (radiant heat): I pass
-
Thermal conductivity (thermal convection): I pass
-
Thermal contact: I class
APPROVE: CCS MED EC SOLAS