Chemical Protective Suits
TYPE:RHF-I
STANDARD
BS EN 14605:2005+A1:2009
OVERALL PERFORMANCE & REQUIREMENT
-
HOOD/COLLAR: Hood fitted with elastic drawtring and chin flap with Velcro. Fits under a safety helmet.
-
On suits with open sleeves, gloves are not included but can be supplied, UVEX rubber glove EN374, EN388
-
On suits with legs, boots are included PVC safety boots, EN 20345, black
-
Nylon zipper on the front protected by a double splash protective flap closing with press studs
-
Material: Polyamide & CR/CSM
-
Weight:330±30g/m²
-
Thickness: 0.27±0.02mm
APPROVE:CCS EC MED SOLAS
Suitable for ships and offshore