Cylinder
Capacity: 0.2L、0.3L、0.35L、0.45L
Safety pressure: 30MPa / 4500psi
Test pressure: 45MPa
Bursting pressure: >80MPa
Tear pressure: 85MPa
Thread specification: M18*1.5, each product has more than 9 teeth, ensuring absolute safety.
Material: 6061 high-precision aluminum (for aviation), high lightness and fatigue resistance.
The product uses 500t high pressure one time molding.
Wall thickness: ≥6MM, thick explosion-proof.
The high temperature thermal healing to prevent any welding.
Flat bottom standard H-type design is uniform, safe and reliable.
Applications: Grass aquarium aquaculture, medical emergency rescue, mountaineering, soda water machine CO2 supply, fire rescue and other occasions.
Detail pictures
Parameter
|
Capacity (L)
|
Safety pressure (MPa)
|
Length * Diameter (cm)
|
Wall thickness (mm)
|
Weight (kg)
|
| 0.2 |
30 |
15*6.1 |
6.3 |
0.55 |
| 0.3 |
30 |
18.5*6.1 |
6.3 |
0.6 |
| 0.35 |
30 |
25*6.1 |
6.3 |
0.8 |
| 0.45 |
30 |
29.5*6.1 |
6.3 |
0.95 |
Size measurement chart